Thanks Mike and Denis,
I don't have any thinking ability this AM and didn't think this subject too
big an issue but for me. Think the spoon in ear stirred grey matter too much.
I like sand blasting but for the sand but acid ain't too cool either. Now,
if Dremel made a miniature sand blasting tool, that would be cool.
Forgot to ask about neutralization when using acids. Is a water rinse
sufficient or must an over 7 ph chemistry be used to do the job?
I know this is a loaded question as well but it must be simple. I've used
the Naval Jelly before and the rinse did the trick. The stuff I'm derusting
is a bit more sensitive and needs as near original surface as possible -
with minimal damage. Some of the surfaces are mildly rusted and others ar a
bit more damaged.
Thanks again,
Earl Moon
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|