Marc
Saponification means making soap. This is done by boiling vegetable
oils, containing fatty acids, with a strong alkali. A chemical reaction
occurs, producing a soap which is water-soluble. As many fluxes contain
carboxylic acids (including rosin) which, like oils, are not
water-soluble. They are therefore reacted with an alkali (usually, but
not exclusively, organic amines) to make them so, and the resultant
"soap" is removed by vigourous water-washing and rinsing. Some, but not
all "no-clean" fluxes are saponifiable. It is a process that needs
careful qualification and process control (the saponifier solution, for
example, requires close temperature control, too hot being just as bad,
or worse, as too cold).
Commercial saponifiers also usually contain organic solvents, to
reinforce the action. As stated, they are highly alkaline and require
good health and safety precautions, especially as the most common active
product, monoethanolamine, is somewhat volatile at the working
temperature and is quite toxic. It is therefore a process to be avoided
by the light-hearted who cannot or will not take the necessary
precautions.
Personally, I recommend water-soluble chemistry over trying to clean
something which is formulated just to avoid the need for cleaning.
E-mail me off-list if you wish more details.
Brian
Marc Cowen wrote:
>
> Hi All,
>
> I am after some advice regarding saponified wash being used with a no-clean
> process.
> What is a saponified wash?
> With regards to not using a wash with a no-clean process is it also common
> practice to use this type of process flow (solder using no-clean flux then
> through a saponified wash).
>
> Thanks for your help.
>
> Best regards
>
> Marc Cowen.
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|