Steve:
Take a look at MIL-S-8516 Sealing Compound, Polysulfide Rubber, Electrical
Connectors and Electrical Systems, Chemically Cured. I think this is more in
line with what you are doing than 8802.
Polysulfde compounds have been around a long time, however for electrical
applications I think most have been replaced by urethanes and silicones.
Good Luck !
Michael Barmuta
Staff Engineer
Fluke Corp.
Everett WA
425-446-6076
-----Original Message-----
From: Stephen R. Gregory [mailto:[log in to unmask]]
Sent: Friday, December 14, 2001 6:26 AM
To: [log in to unmask]
Subject: [TN] Alumina filled Polysulfide compound...
Hi All!!
...tappity-tappity-tappity...(doin' my thank gawd it's Friday dance! hehehe)
I was wondering if someone could point me in a direction where I could find
some alumina filled polysulfide compound, per MIL-S-8802, class A-2, with 50
plus or minus 10%, 325 mesh aluminum oxide powder...
This is something that is called out on a drawing for a board that's using
this material to strain relief two small battery cables that are installed
on the board...I've searched and find a bunch of stuff about polysulfide
compounds, but nothing alumina filled. If I search under MIL-S-8802, I find
all kinds of polysulfide sealers for jet fuel tanks, but still nothing
alumina filled...
Any help will be much appreciated
-Steve Gregory-
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|