TECHNET Archives

December 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Hinners Hans M Civ WRALC/LUGE <[log in to unmask]>
Date:
Fri, 14 Dec 2001 09:24:20 -0500
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Parts/Attachments:
text/plain (66 lines)
Hi Phil,

We solved this problem by color coding the flux bottles and placing a
colored sticker on the work control document.  Without it folks were using
whatever was in-front of them.  Extra instructions alone didn't work.

Hans

Integrity First  -  Service Before Self  -  Excellence in All We Do
~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~
Hans M. Hinners
Electronics Engineer
Warner Robins - Air Logistics Center (WR-ALC/LUGE)
226 Cochran Street
Robins AFB GA 31098-1622

mailto:[log in to unmask]

Com: (478) 926 - 5224
Fax:   (478) 926 - 4911
DSN Prefix: 468


-----Original Message-----
From: [log in to unmask]
[mailto:[log in to unmask]]
Sent: Friday, December 14, 2001 8:05 AM
To: [log in to unmask]
Subject: [TN] Flux Controls


Hello Technetters

I need help. Currently I have only RMA fluxes in wave soldering and hand
soldering. We are planning to use type QA for a new customer.  I am
concerned about what kind of controls I should have in place so the right
flux is used only on the assemblies that it is intended.

Thanks in advance.
Phil Belliveau

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2