TECHNET Archives

December 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
David Hillman <[log in to unmask]>
Date:
Wed, 12 Dec 2001 08:59:58 -0600
Content-type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Parts/Attachments:
text/plain (60 lines)
Hi Andre! One of my mentor's always used to tell me that the theme song for
components which do not incorporation stress relief in the lead
configuration was "Pop goes the Weasel"! In fact he used to hum the tune
during design/producibility reviews. No stress relief is a bad idea unless
you like cracked solder joints or damage components.

Dave Hillman
Rockwell Collins
[log in to unmask]





Andre Leclair <[log in to unmask]>@ipc.org> on 12/12/2001 07:25:59 AM

Please respond to "TechNet E-Mail Forum." <[log in to unmask]>

Sent by:  TechNet <[log in to unmask]>


To:   [log in to unmask]
cc:

Subject:  [TN] To form or not to Form


Hi all
I hope this gets some good advice.

I have a customer who is requiring the placement of an electrolitic cap
that has a lead spacing of 0.140" and the PCB has 0.100".  They do not want
the leads formed, they want the part flat to the board.  In doing this, am
I opening myself up to stress induced failures of the component.

---------------------------------------------------------------------------------

Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2