TECHNET Archives

December 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Date:
Tue, 4 Dec 2001 00:40:08 +0100
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Content-type:
text/plain; charset=ISO-8859-1
Subject:
From:
Matthias Mansfeld <[log in to unmask]>
Content-transfer-encoding:
Quoted-printable
MIME-Version:
1.0
Organization:
Matthias Mansfeld Elektronik
Comments:
Authenticated sender is <[log in to unmask]>
Parts/Attachments:
text/plain (38 lines)
Hello all,

A customer of mine wanted to simulate the heat dissipation within a
board (burn-in and test boards for CSP) and thus I tried to get these
values for some high-Tg materials. All I found was 0.3 W/(m*K) für
some Arlon materials (88N). They refer to a ASTM E-1225 method.

My questions:

I would assume, there is a different thermal conductivity in x/y and
z direction for any substrates with E-glass inside. Where can I find
such values? Which test method would be appropiate?

Has anybody a short summary/comparison or a good WWW link about the
different (mostly ASTM) methods and their pros and cons?

Has anybody made such thermal conductivity measurements especially
for G30 or P95 or Duraver PD or Arlon 35N, all in 0.8 mm thickness,
18 um copper and would be willing to share the results?

Thanks a lot, best regards
Matthias Mansfeld
-----------------------------------------------
Matthias Mansfeld Elektronik
* Leiterplattenlayout, Bestueckung
Am Langhoelzl 11, 85540 Haar; Tel.: 089/4620 093-7, Fax: -8
Internet: http://www.mansfeld-elektronik.de

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2