We've found sodium silicate particles on equipment due to over application
of floor sealant. I'm looking for information regarding if it will effect
our equipment performance either electrically or mechanically, or the health
of employees who use it. If a complete cleaning is necessary, what would be
the best way to remove the sodium sulfate contamination without damaging our
equipment?
Jennifer
-----Original Message-----
From: <Rudy Sedlak> [mailto:[log in to unmask]]
Sent: Tuesday, December 11, 2001 10:13 AM
To: [log in to unmask]
Subject: Re: [TN] Sodium Silicate Contamination
Jennifer:
Allow me to ask why you are interested, and where you have the potential for
contamination by Sodium Silicate.
Sodium Silicate is a very common ingredient in water based alkaline (read
this as high pH) detergents, and is commonly used as an anti-tarnish,
anti-corrosion agent in these detergents. Most machine dishwashing
compounds
have sodium silicate in them.
It can cause problems if the pH of the cleaner gets too low, as it always
does in a rinse. It can also cause problems in high water hardness, where
it
reacts with the water hardness, and falls out of solution as typically
Calcium Silicate.
And even if you have enough water softener in the detergent to overcome the
hardness in the cleaner itself, in the rinse you can still generate Calcium
Silicate.
My recommendation is to avoid Sodium Silicate in general, unless you have a
well formulated product with enough water softeners, and a good,
non-recirculating rinse.
Rudy Sedlak
RD Chemical Company
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|