Hi Jorge,
>All the thermocouples were directly attached to the component solder joints,
the
>peak temperature reaches 210 degrees Celsius. The time above liquiduos
(183C) is 60 >seconds. The component is a 0.020" pitch plastic QFP, the body
>measures around 30 mm by 30 mm. I'm quite sure the profile numbers are
>right, it works for everything on the board, but those QFPs. No idea what's
>wrong. Any ideas of what may be happening?
ANSWER: Well, this comes from some of the technically sloppy ideas that float
around in the industry. 60 seconds above 183C is not necessarily enough for
some components, and certainly not with a higher melting solder like you have
on your leads. In order to get reliable reflow you need to be at or higher
than [Liquidus + 20C] for about 5 to 10 seconds. At a peak reflow temperature
of 210C you are nowhere near that. Also for larger components like this you
need to attach the thermocouple to a non-soldered lead notone that is already
attached to the PCB--the component interior is a heat sink.
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 386-437-8747, Fax: 386-437-8737
E-mail: [log in to unmask], Website: www.engelmaier.com
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|