Peter,
Have you checked PTH in your boards for barrel plating quality?. Many times blowholes are
caused by out gassing from the laminate through plating voids. A micro section of PTH showing
blowholes will be very helpful.
PL wrote:
> Hello,
>
> I would like to ask your input on trouble shooting a wave soldering
> process that I've encountered producing blow holes on the PCA. The blow
> holes were seen at random locations, mostly on small and light caps. The
> boards were manufactured in recent weeks. Some board warppage was
> noticed after the wave.
>
> Things I tried:
> - Boards from a different manufactured date, no effect
> - Turned on turbulence wave. It reduced but didn't completely eliminate
> the defect
> - used stiffener on board edge to reduce board sagging
> - used dummy weights on top of parts seen having defect to minimize
> "dancing" during wave
>
> How critical is the component lead-to-hole ratio as far as its impact on
> solder joint quality?
> Could anyone explain how a blow hole can occur and possible steps taken
> to eliminate the defect?
>
> Rgds,
> Peter
>
> _________________________________________________________
> Do You Yahoo!?
> Get your free @yahoo.com address at http://mail.yahoo.com
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
--
_________________________
pratap singh
tel/fax: 512-255-6820
email: [log in to unmask]
WEB: www.rampinc.com
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|