Continuing with a previous posting, Amkor uses the following pad to ball
size [mm] relationship:
Package||PBGA||PBGA||PBGA||SuperBGA||SuperBGA||fleXBGA ||fleXBGA
Pitch||1.5||1.27||1.0||1.27||1.0||1.0||0.8
Ball diameter||0.76||0.76||0.50||0.76||0.63||0.45||0.45
Pad size||0.63||0.63||0.45||0.63||0.55||0.45||0.30
IPC-7095 suggests the ball size reduction approach that a couple of others
mentioned
Nominal Ball Size ||Reduction||Nominal Land Dia||Variation
0.75mm ||25% ||0.55mm ||0.60-0.50mm
0.60mm ||25% ||0.45mm ||0.50-0.40mm
0.50mm ||20% ||0.40mm ||0.45-0.35mm
Dave Fish
----- Original Message -----
From: "Genny Gibbard" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, November 06, 2001 7:24 AM
Subject: [TN] BGA's in design
> OK, in the next few months we will probably design our first board that
uses
> a BGA, and we are jumping in with both feet. This board will have a 304
> ball 1.27mm pitch, a 432 ball 1.27mm pitch, a 196 ball 1.00mm pitch and a
> 256 ball 1.00mm pitch.
> Are there any resources for free land patterns for these babies? Or how
do
> you determine the pad size knowing the ball diameter and pitch? Almost
> every place I found on the web with BGA patterns was selling them. I was
> looking at the table of contents for the SM-782A standard and it only
> mentioned 1.27pitch. Is the information in the standard easily scalable
to
> smaller pitch? It could be a hard sell to convince my company to buy
> patterns, which means we will probably make our own which doesn't always
> make for very good DFM.
> Secondly, (I hesitate to ask this, because I may get a bunch of
> solicitations, but) does anyone have some recommendations for board
> fabricators in Canada that can handle the BGA requirements? We have had
> questionable quality from most or all of our current board vendors at some
> time or another (remember the switched inner layers?) and I am looking
for
> some new sources.
>
> Regards.
>
> Genny Gibbard (mailto:[log in to unmask])
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|