After a brief 3.5 day trip from BF Montana to Eastern Michigan, I'm back.
Big whoop! How 'bout those Chicago commuters! Never again as long as I live
will I take the 80 anywhere near that city. Trains only, thank you.
You measure the amount of oxygen (%), not the nitrogen purity or amount -
can't be done. The oxygen content should be as specified for the type
soldering you are attempting. Usually, below 20% oxygen content is acceptable.
MoonMan
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|