Our std at BAE Systems was 90 deg C (194 F) for 1 hour, though since I have
achieved greater enlightenment, I would suggest that you have your boards
packed by your fab house in sealed bags with desiccant, you keep them in a
dry cabinet and that you don't open them until needed on the line. That way
you won't have to pre-bake them, and they won't have to go through an
avoidable thermal excursion.
Peter Duncan
Rick Howieson
<RHowieson@DELTAGRO To: [log in to unmask]
UPINC.COM> cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST
Sent by: TechNet Aero/ST Group)
<[log in to unmask]> Subject: [TN] Pre-bake
11/20/01 01:41 AM
Please respond to
"TechNet E-Mail
Forum."
What is the recommended pre-bake of multilayer boards prior to insertion
and
wave. 221F for 1hour??? Or would this be a little extreme?
Thanks,
Rick
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|