Jim, Remember the Solder Pots we used for Tinning Wires? It works great for
stripping the insulation of the Magnet Wire.
-----Original Message-----
From: Marsico, James [mailto:[log in to unmask]]
Sent: Wednesday, October 31, 2001 1:11 PM
To: [log in to unmask]
Subject: Re: [TN] STRIPPING MAGNET WIRE
Can't find ant info on Beck chemicals (EPOXYSTRIP T-251-C) or Insulstrip
Jell. Do you have any additional information?
Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879
-----Original Message-----
From: Matt Stanik [SMTP:[log in to unmask]]
Sent: Wednesday, October 31, 2001 12:46 PM
To: [log in to unmask]
Subject: Re: [TN] STRIPPING MAGNET WIRE
Beck Chemicals of Cleveland, Ohio used to sell a product called
EPOXYSTRIP T-251-C specifically for removing insulating varnishes
and epoxies from wire and such. It worked great.
> Looking for a recommendation for a chemical stripper to strip
bi-filar (?)
> magnet wire. Any suggestions?
>
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following
text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message:
SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
----------------------------------------------------------------------------
-----
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|