Insulstrip Jell stripper for Magnet wire insulation:
Ambion Corporation
37 Naugatuck Drive
Naugatuck, CT 06770
(203) 723-1437
I called to verify that they still handle this chemical.
-Sherry
>Can't find ant info on Beck chemicals (EPOXYSTRIP T-251-C) or Insulstrip
>Jell. Do you have any additional information?
>
>Jim Marsico
>Senior Engineer
>Production Engineering
>EDO Electronics Systems Group
>[log in to unmask] <mailto:[log in to unmask]>
>631-595-5879
>
>
>
> -----Original Message-----
> From: Matt Stanik [SMTP:[log in to unmask]]
> Sent: Wednesday, October 31, 2001 12:46 PM
> To: [log in to unmask]
> Subject: Re: [TN] STRIPPING MAGNET WIRE
>
> Beck Chemicals of Cleveland, Ohio used to sell a product called
> EPOXYSTRIP T-251-C specifically for removing insulating varnishes
> and epoxies from wire and such. It worked great.
>
>
> > Looking for a recommendation for a chemical stripper to strip
>bi-filar (?)
> > magnet wire. Any suggestions?
> >
>
>
>----------------------------------------------------------------------------
>-----
> Technet Mail List provided as a free service by IPC using LISTSERV
>1.8d
> To unsubscribe, send a message to [log in to unmask] with following
>text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message:
>SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources &
>Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
>additional
> information, or contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>
>----------------------------------------------------------------------------
>-----
>
>---------------------------------------------------------------------
>------------
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt delivery of Technet send the following message:
>SET Technet NOMAIL
>Search previous postings at: www.ipc.org > On-Line Resources &
>Databases > E-mail Archives
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information, or contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>---------------------------------------------------------------------
>------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|