George,
Circuit Technologies
Haverhill, Mass.

If they can't do it, no one can.
Good Luck

-----Original Message-----
From: George Becker [mailto:[log in to unmask]]
Sent: Friday, November 09, 2001 8:41 AM
To: [log in to unmask]
Subject: [TN] Thick PCBs


Occasionally I have been asked if there is some type of mechanical repair
process for PCBs with edge contacts that exceed the thickness measured at
the contacts.  I have heard that there is a process to machine out an edge
'kerf,' squeeze the PCB down to size and epoxy it to required thickness.
Does anyone perform this type of repair?  Where can I find out info. on
this?
Is there any method that has been tried and was successful which uses
pressure (like from a press) to squeeze edge metallization down? (This
pressure method would appear to be less intrusive than the machining method
above since the board is not cut.)

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2