Many components have an organic coating on the tin-lead. I recommend a
good clean in a strong saponifier cleaning process, followed by a couple
of hours or so at 80-100°C.
Brian
Julien Bouchard wrote:
>
> Hi,
> We implement a more structured training program and in a part of this
> programs, we want to train the operator by give them pratice on oxidized
> tin-lead plated component. Does someone know a way to accelerate the natural
> oxiditation process of tin-lead alloys using in electronic to simulate and
> heavily oxidized component ? Thank.
>
> Julien Bouchard ing. stag.
> Matrox - Process Engineer
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|