Hey all,
I anyone using an Electrovert Minipak 300 wave soldering machine??? I have
one we use occasionally for smaller products/prototyping for various
customers, and I am keen on finding out the average pre-heater temperatures
people are using. I have only recently descovered, that ours is set at
around 600 degrees F. This seems very high to me, does anyone have any
comments???
Cheers
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|