We use Conceptronic Freedom2000 and it does a reasonable job. Generally,
one tries to imitate the profile used for placement. The Conceptronic helps
establish the profile but you must embed up to 4 thermocouples in a scrap or
dummy board in order to accurately establish the time/temperature profile
you need. The computer will store many profiles and there are two access
levels to allow the repair operator to access the engineer-established
profiles but not change them. The repair station will display the profile
graphically.
George Carroll
Process Engineer
Siemens Energy and Automation
Johnson City, TN
[log in to unmask]
-----Original Message-----
From: Vaishnav, Bankim [mailto:[log in to unmask]]
Sent: Wednesday, November 07, 2001 3:51 PM
To: [log in to unmask]
Subject: [TN] BGA rework
Any thoughts on better auto / semi auto BGA rework equipment to use - SRT,
AIRVAC, PACE or any other available.
Also, about profiling for removing and replacing BGA from the Bonded
assembly / chassis assembly. Is it generally done or need to remove board
assembly from boded assembly / chassis assembly first prior to BGA rework.
Bankim
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|