Technetters,
We've been having some issues for a while with some QFPs coming with
85/15 leads, the solder doesn't flow properly, not very nice heel fillet.
Does anybody has recommendations as far as the reflow profile?. I read
somewhere that this particular alloy has the liquidus temperature at 205
degrees, is this accurate?
Thanks for the feedback
Jorge Rodriguez