Michael,
For high purity conductive epoxies with low ionics try Ablestik (subsidiary
of National Starch and Chemical Company) or Epotek.
Regards,
Bruce Misner
> ----------
> From: Michael Bell[SMTP:[log in to unmask]]
> Reply To: TechNet E-Mail Forum.
> Sent: Monday, November 05, 2001 7:39 PM
> To: [log in to unmask]
> Subject: [TN] Electrically Conductive Epoxies
>
> Hi all,
>
> Has anyone got any feed back on Electrically Conductive Epoxies??? I am
> looking at Loctite 3888 but I am unsure whether this is a very good, does
> anyone know of any other reputable brands/types???
>
> Cheers
>
> --------------------------------------------------------------------------
> -------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
> Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> --------------------------------------------------------------------------
> -------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|