How about our afvourite IMC's building up within the component -
ball/component interface for example? Will that affect long term
reliability/solderabity after a long period of storage?
Just thought I'ld throw that one into the pot.
Peter Duncan
"d. terstegge"
<[log in to unmask] To: [log in to unmask]
GROUP.COM> cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST
Sent by: TechNet Aero/ST Group)
<[log in to unmask]> Subject: Re: [TN] BGA long term storage?
11/28/01 07:08 PM
Please respond to
"TechNet E-Mail Forum."
Hmmm, seems I'm the only one who adviced not to worry about long term
storage of BGA's. I must admit that I never stored a BGA for 10 years to
see how it solders, but I really don't expect the solderability to decrease
to such an extend that the balls will not solder anymore.
According to Klein Wassink the oxidation layer on solder will grow
approximately logarithmically with time, resulting in about 6nm after 20
years which is just twice as thick as after one year !
So my question is: are nitrogen cabinets, ROSA-technology or redesigns
REALLY necesarry ?
Maybe one of the metallurgists on this forum can add a few words ?
Daan Terstegge
SMT Centre
Thales Communications
Unclassified mail
Personal Website: http://www.smtinfo.net
>>> Graham Collins <[log in to unmask]> 11/27 1:02 pm >>>
Hi Doug!
Indeed - not a new problem - and one we have faced on other programs. It's
just the BGAs that are new to us for this problem.
Nitrogen storage is available here and I expect that's what we will use
(unless some other TechNet guru has a better idea!).
I've heard of ROSA, and in fact Dave was kind enough to send me a 35mm
thick document describing some experiments and results with it. Very
interesting machine. Do you know if anything ever come of the work to
produce a commercial (non-lab) version of this? Hmm... wonder what
happened to Bev's?
Anyway - thanks to everyone for the responses. Nitrogen storage was/is the
plan, but it is always good to have a sanity check with some experts.
regards
Graham Collins
Process Engineer,
Northrop Grumman
Atlantic Facility of Litton Systems Canada
(902) 873-2000 ext 6215
>>> [log in to unmask] 11/26/01 04:11PM >>>
The issue of long term storage of parts or boards is not a new one. The
military, faced with REALLY long lifetimes (e.g. 50 years for a MX missile)
and decreaseing market clout, has had to deal with lifetime buys for a long
time. In my mind, there are two possibilities: (1) preserve the original
solderability for as long as possible, or (2) plan on restoring the
solderability at some point in the future when the part is needed.
In the first case, you will have to setup some fairly elaborate storage
conditions where oxygen and moisture are excluded. Dry nitrogen is most
common, but alternatives could include dessicated conditions or coverage
with a heavy noble gas like argon. You will have to setup incoming and
outgoing logs that tightly control the inventory, and you have to have
floor space for the storage for the life span of the part.
In the second case, you restore the solderable surface. Some people do
this using aggressive fluxes and re-tinning, with limited success. An
alternative to this is to use an electrochemical reduction process called
ROSA to change the surface oxides to the base metal, restoring
solderability. ROSA can be done on many parts at the same time, it is
electroless, and is not too capital intensive. Dave Hillman of Rockwell is
the master of ROSA and has published a number of papers on the topic. He
would probably answer more fully but he is currently putting the finishing
touches on his Master's thesis and so won't stick his head out of his
cubicle for another few days. And when he does, if he sees his shadow,
there will be 5 more months of winter (in Iowa, that's a safe bet). Where
was I?
The advantage of the ROSA approach is that it does not matter all that much
what the solderability condition was when the part was received, and the
storage conditions do not have to be draconian.
As the commercial goes, you can pay me now or pay me later.....
Doug Pauls
Rockwell Collins
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|