TECHNET Archives

November 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
"<Rudy Sedlak>" <[log in to unmask]>
Date:
Mon, 26 Nov 2001 20:31:46 EST
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Parts/Attachments:
text/plain (20 lines)
If Mark Mazzoli's graph is not good enough....Don Ball of Atotech (formerly
Chemcut) in State College PA has a graph on data he generated with his own
hands...

Remember, that absolute etch rate is also a function of ORP, so one man's one
normal acid etch rate may not be the same as your results.

Rudy Sedlak
RD Chemical Company

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2