Hi Graham,
Long term storage is more a problem for QFP's and other leaded parts, where intermetallics can make the parts unsolderable.
The oxidation that you will have on the BGA's balls is what you're using flux for. I don't think you will have any soldering problem at all, as long as you bake before soldering.
Daan Terstegge
SMT Centre
Thales Communications
Unclassified mail
Personal Website: http://www.smtinfo.net
>>> Graham Collins <[log in to unmask]> 11/26 4:07 pm >>>
Good day Technet! Hope my friends to the south had a good Thanksgiving holiday!
A question today concerning shelf life and storage. We build equipment that is expected to be supported for a fairly long time - say a decade or more. We are also as an industry moving to using COTS (commercial) components to reduce cost. Fine and good, but the life cycle for commercial parts is often pretty short compared with a military spec'd component - which puts us into a life time buy situation earlier rather than later.
My question:
Is there a good method to use to store BGA type components for long term storage? E.G. I build board X using a particular BGA part. It goes "end of life" a couple of years later, but I'm expected to support repair and overhaul for another few years yet, so I buy as many as I predict I'll need. As the time goes on, the solder balls oxidize. How should I store the spare parts? In nitrogen? Cold environment? Will it even be a problem?
regards
Graham Collins
Process Engineer,
Northrop Grumman
Atlantic Facility of Litton Systems Canada
(902) 873-2000 ext 6215
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|