TECHNET Archives

November 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
"<Peter George Duncan>" <[log in to unmask]>
Date:
Fri, 23 Nov 2001 12:15:34 +0800
Content-type:
text/plain; charset=us-ascii
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Parts/Attachments:
text/plain (130 lines)
Hi, Ian,

I've attracted a remarkable amount of correspondence on this subject, and
have been very impressed with the help and information received. Laser
drilling is brand new to me, and with everyone's help, I feel I'm building
up a pretty comprehensive overview of this technology, which is very
interesting learning. It's a tricky process, it seems in inexperienced
hands, but for people who know it, they say it's every bit as reliable as
more conventional methods and much cheaper. Hopefully we won't have too
many projects that require it, unless we do find a fab house at the right
price who can successfully handle all the processes.

On the grinding thang, your concern was exactly mine when it was first
proposed by the fab house - by grinding off the plated copper, I'ld be left
with plated copper joined to the inside thickness of the original pad. I've
seen enough microsections in my time to know that there is a "weakness" at
the interface of these two metalisations. Although there is a final plating
session that will cover a lot of this, still it is a concern.

Thanks again to you and all the others who have responded on this issue. I
hope it's helped more people than just me.

Best regards

Peter Duncan







                    Ian Hanna
                    <ianh@LAZER-T        To:     [log in to unmask]
                    ECH.COM>             cc:     (bcc: DUNCAN Peter/Asst Prin Engr/ST
                    Sent by:             Aero/ST Group)
                    TechNet              Subject:     Re: [TN] Over-etch
                    <[log in to unmask]
                    ORG>


                    11/22/01
                    09:49 PM
                    Please
                    respond to
                    "TechNet
                    E-Mail
                    Forum."






just a quick note on lasing...i found it, once dialed in, to be a very good
process.  the biggest deal besides ablating the holes is plating
them...sounds like an old song now.  it took me less than a week to work up
a very wide process window for 1080 fr-4 with an nd/yag UV laser.
everything looked great on the microsections but we found we had about .5%
fall out due to plating voids in the finished boards...a difficult number
to
really work with, too slim for easy failure analysis yet one or two opens
per board didn't work...used really low amps and a couple of 'cheats' at
electroless (metalization) to get the job out...and ended up going to
complex waveform reverse pulse plating...which made things more or less a
cake-walk...bottom line is that if i was to bring laser drilling in house
again i'd sub-contract the drilling (that is hold off on the rather
substantial capitol investment in a laser via machine) until i had the rest
of my processes dialed in...registration on n-1 layers...coordinating the
registration between the mechanical hole grid and the micro-via
placement...and of course reliable process....one of the more 'holistic'
processes i've worked with...everything needs to work together, you can't
just ship out panels for drilling and process them the same old way...

might as well throw in my $.02 worth on your grinding idea....i'm a little
concerned about the integrity of the 'knees' of the plated barrels...it's
always nice to see an even coating of rich, thick, well leveled copper
going
from the surface all the way into the barrel of the hole...interrupting
this, then re-plating over top -might- not give you as solid a 'knee' and
with board expansion from z-axis CTE mismatches so common in fr-4
construction, you might see a higher than normal drop out well after the
fabrication fact...i'd do some fairly aggressive solder floats, at least 5x
10 seconds in a pot of 550 degrees and look for any signs of failure...to
ensure that there are no long-term reliability issuesthat being said,
i've plated, filled and ground lots of blind vias without too many
reliability issues in avionics applications...so it's do-able...just so
you're aware of potential pit-falls really...


good luck...sounds like an exciting project



ian

---------------------------------------------------------------------------------

Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------





[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2