In a message dated 11/20/01 2:40:04 PM Pacific Standard Time,
[log in to unmask] writes:
Steve:
Do not know if this roughness is a problem, as that ain't my area of
expertise, (if I have one....) but, the "The roughness seems worse in the
smaller diameter holes than do the larger holes" statement yells that the
problem is caused by gas bubbles trapped in the holes....and thus could
probably be remedied (minimized) by "canting" or tipping the boards during
Nickel plating, to allow the bubbles to come out of the holes.
Rudy Sedlak
RD Chemical Company
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------