TECHNET Archives

November 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Earl Moon <[log in to unmask]>
Date:
Sat, 3 Nov 2001 07:22:00 -0600
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Parts/Attachments:
text/plain (43 lines)
Folks,

Especially with JK's help during my GaAs FA adventure, a few weeks ago, I
was able to determine many interesting factors concerning the use of
MIL-STD-883E's test method 2030. It provides details about using C-SAM
(scanning acoustic microscopy), to visually determine voiding, and gives
graphic acceptance criteria, in percent voiding in, primairly, eutectic and
adhesive bonding of semiconductor devices to whatever substrate required.

This method, and its criteria, is derived, I presume, from data correlating
voiding percentages to thermal conductivity efficiency and effectiveness.
However, it does present some drawbacks.

As I am preparing to use the same method, or something better if available,
do study the effects of various thermal adhesives used to mount RF
amplifiers, and various other device types, to a cold wall. The experiments
must show the relationship of such voiding in selected adhesives to thermal
conductivity. The experiments are straighforward enough. However, the
problem is: it is really hard some times, using C-SAM, as an example, to
really "see" and quantify the voiding percentage amounts. I need assistance
in using a better test method (didn't do well with x-ray on previous
occassions), if available, to better "see" and correlate findings.

All help appreciated.

Earl Moon


Also, I meant to say smooth side facing in toward preg on the issue of
capacitance planes.

Thanks

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2