Hi Grant,
that´s the trouble with customer supplied components. If you don´t know the
history of that package and the devices in respect to moisture and open time
baking should be the way to go.
Your approach to get those parts in the normal workflow for MSD-parts using
drybacks and recording the history sounds reasonable and you should convince
your customer of the merits of these procedures. In future you may not have
to bake his components.
Good luck
Wolfgang
-----Ursprüngliche Nachricht-----
Von: Grant Emandien [mailto:[log in to unmask]]
Gesendet am: Donnerstag, 15. November 2001 10:16
An: [log in to unmask]
Betreff: [TN] Handling of moisture sensitive devices
Hi All,
I am seeking advice on handling methods of moisture sensitive devices from
reception/storage to use. Components have varying baking requirements after
the packaging has been opened - is baking performed as per. manufacturer's
instructions?
One of our customers is insistent on us, as an assembler to bake
(customer-supplied) components just prior to assembly - this approach
however does impose some impracticalities on production. Our initial counter
proposal is to receive only components in original OEM wrapping indicating
the moisture instructions and class/level and to then return bake and reseal
(vacuum/nitrogen) excess opened material to stores - the package would also
include a humidity indicator. Our proposal is more amenable to production,
but is it sufficient to ensure device integrity? Any insights on the
approach of assemblers?
TIA
Grant
**********************************************************************
Notice:
The information contained in this e-mail (including any attachments) may
contain commercially sensitive or confidential information which may be
legally privileged and is for the sole use of the intended recipient(s). If
you are not, or believe you may not be, the intended recipient, you are
hereby notified that any use, dissemination, copying, review, disclosure or
action taken in reliance of this e-mail is prohibited and may be unlawful.
If you have received this message in error, please notify the sender
immediately by reply e-mail and delete all copies of the message.
Any views expressed in this message are those of the individual sender
unless expressly stated by the sender to be given on behalf of Tellumat
(Pty) Ltd. Tellumat (Pty) Ltd disclaims liability for any unauthorised
opinion or representation made by the sender on behalf of Tellumat (Pty)
Ltd.
No warranty is given by Tellumat (Pty) Ltd that the integrity or security of
this e-mail (including any attachments) has been maintained through
transmission, nor that the communication is free of virus, interception or
interference.
**********************************************************************
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|