/Dear all,
I'm looking for some advice on the threshold limits for solder temperatures,
if for example, HMP solder is solidus/liquidus at say 296-301 deg C, what is
the highest temperature excursion it can see in service before the
properties of the soldered connection are affected?
I heard somewhere that as a rule of thumb you should allow around 40 deg C
below the melting point of the solder being used.
Any help/advice that you can give would be appreciated.
regards,
Pat Diamond
Weston Aerospace
Farnborough
UK
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|