Genny,
A lifetime ago I was involved with a solder leveling system called
the Lightning. It involved immersion fluxing/preheating the panel, then
immersing it in a pot of molten solder, then using an immersion hot oil with
liquid knife technology to squeegee the excess solder off the pads and out
of the holes. Theoretically a system easier to control than air since you
were working with a heavy liquid than a compressible gas. THEORETICALLY!
It was extremely dirty and dangerous, and you wouldn't want to go
there.
Greg Anderson
Senior Advanced Manufacturing Engineer
GE Fanuc Automation
Charlottesville, VA 22911
Phone: 434-978-5181
FAX: 434-978-5898
e-mail: [log in to unmask]
-----Original Message-----
From: Genny Gibbard [mailto:[log in to unmask]]
Sent: Friday, November 09, 2001 12:27 PM
To: [log in to unmask]
Subject: [TN] Hot Oil
You learn something new (or new to you) every day.
I was just told of a board finishing process called Hot Oil Solder
Levelling. It was portrayed as a very flat, nice finish. I was also told
that it is old technology, which may be why I am not familiar with it. It
is only within the last year that I have really gotten involved with
specifying board finishes. I've been searching on the internet to learn
more and am a bit confused.
My questions:
Is Hot Oil Reflow and Hot Oil Surface Levelling the same thing? If not,
what is the difference?
What are advantages/disadvantages to this over HASL, or any of the newer
so-called 'flat' finishes needed for fine pitch?
Thanks.
Genny Gibbard (mailto:[log in to unmask])
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|