Cheryl:
Be aware that most "chloride" measuring devices/systems simply measure
conductivity, and express it as equivalent amounts of Sodium Chloride, so
they really do not actually determine chloride, they determine conductivity.
And anything ionic can contribute to conductivity, and that can come from
either flux or tap water.