Mike,
Enlarging the corner pads would seriously affect co-planarity. A better
approach seems to be to eliminate the corner pads. Many manufacturers are
doing this.
Bruce Misner
> ----------
> From: Yuen, Mike[SMTP:[log in to unmask]]
> Reply To: TechNet E-Mail Forum.
> Sent: Wednesday, October 17, 2001 10:59 AM
> To: [log in to unmask]
> Subject: [TN] BGA corner pad
>
> Greetings,
>
> I understand BGA reliability is a very complex subject. Folks had been
> doing DOEs for years trying to determine the significant factors
> involved. For most perimeter PBGA, corners joint seem to be the weakest
> link. I wonder if anyone out there had done studies on enlarging just
> the corner pads of a BGA to enhance reliability.
>
> Thanks,
> M. Yuen
>
> --------------------------------------------------------------------------
> -------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
> Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> --------------------------------------------------------------------------
> -------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|