I understand BGA reliability is a very complex subject. Folks had been
doing DOEs for years trying to determine the significant factors
involved. For most perimeter PBGA, corners joint seem to be the weakest
link. I wonder if anyone out there had done studies on enlarging just
the corner pads of a BGA to enhance reliability.
Thanks,
M. Yuen
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|