We had, on occasion, had to solder additional copper foil (solder coated)
from the filters to ground. Maybe this is an option.
Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
631-595-5879
-----Original Message-----
From: Jim Kittel [SMTP:[log in to unmask]]
Sent: Thursday, October 11, 2001 11:27 AM
To: [log in to unmask]
Subject: [TN] Attaching Microwave Components
Hello Tec Netters,
We are de-buging a new circuit board containing a microwave filter
operating
in the 2 - 3 Ghz range. This filter was soldered around the
perimeter of
the case to the ENIG ground plane using 63/37 eutectic. The
engineer is
stating that electrically the filter does not appear to be
adequately
grounded to that plane. I am wondering if there is a better way to
attach
these filters? Would it be better to solder the entire bottom of
the filter
case to the plane? Is anyone using conductive epoxy? Liquid or
sheet? I
would appeciate comments.
Thanks,
Jim Kittel
L-3 Communications
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following
text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message:
SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|