Do you know the the 3M part no# for this tape? I am very intrested to see if
it help with a problem i have
thankyou
JOE KEARY
-----Original Message-----
From: Eric Christison [mailto:[log in to unmask]]
Sent: Monday, October 01, 2001 3:14 AM
To: [log in to unmask]
Subject: Re: [TN] Flex and Soldering
We attach a flex to a ceramic substrate using a hot bar BUT using a 3M Z
axis adhesive tape.
The flex has very closely spaced pads and these were prone to shorting when
we tried hot bar soldering. We also found the adhesive gave a stronger joint
mechanically.
However cycle time for hot bar - whether solder or ACF - is not that good. I
would suggest about 1 minute per joint and it is done manually although a
certain amount of automation is possible.
One very large phone manufacturer told me the other week that they
absolutley loathe the hot bar process. A yield hit of 8% on a million phones
a month gets your name in the corporate spotlights...
Hope this helps,
> Technet,
>
> Does anyone have any guidelines for soldering flex circuit directly to a
> PWB? We currently connect it mechanically and with a connector, but
> were toying with the idea of direct solder attach.
>
> Any experience, do's and don't, especially horror stories, appreciated.
>
> Thanks......DT
>
>
>
Eric Christison
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|