Steve,
I've seen images like this long ago. . . caused then by rework of solder
mask. Most things that strip solder mask also do a number on the "butter
coat". Shows up first at the thinner "knuckle" of the glass weave.
Greg Anderson
Senior Advanced Manufacturing Engineer
GE Fanuc Automation
Charlottesville, VA 22911
Phone: 804-978-5181
FAX: 804-978-5898
e-mail: [log in to unmask]
-----Original Message-----
From: Stephen R. Gregory [mailto:[log in to unmask]]
Sent: Tuesday, July 17, 2001 9:56 AM
To: [log in to unmask]
Subject: [TN] Weave Exposure...
Hi Everyone!
I've got some boards in here that has what I believe to be weave exposure,
and I think it's bad enough to reject the boards. Go to:
http://stevezeva.homestead.com/index.html
and tell me what you think. What causes something like that?
-Steve Gregory-
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|