Mike,
Folks at Nokia Research Center in Irving, Texas did studies on enlarged
corner pads. They were trying to improve PBGA reliability without using
underfill and found that removing the corner solder joints didn't help much.
Their other option was to strengthen the joints by making the balls
oversize. By making the corner pads and balls bigger, they anchor the
package to the carrier and are better able to handle shock inputs. Their
solution was dubbed "anchor pads."
Let me know if you would like more info.
Terri
> ----------
> From: Yuen, Mike[SMTP:[log in to unmask]]
> Reply To: TechNet E-Mail Forum.
> Sent: Wednesday, October 17, 2001 10:59 AM
> To: [log in to unmask]
> Subject: [TN] BGA corner pad
>
> Greetings,
>
> I understand BGA reliability is a very complex subject. Folks had been
> doing DOEs for years trying to determine the significant factors
> involved. For most perimeter PBGA, corners joint seem to be the weakest
> link. I wonder if anyone out there had done studies on enlarging just
> the corner pads of a BGA to enhance reliability.
>
> Thanks,
> M. Yuen
>
> --------------------------------------------------------------------------
> -------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
> Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> --------------------------------------------------------------------------
> -------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|