Are the capacitor locations properly thermal relieved? What is the orientation into the wave at this location? Could it be that the part is being thermally shocked due to lack of stress relief in the PCB or orientation into the wave?
Kathy
<!DOCTYPE HTML PUBLIC "-//W3C//DTD HTML 4.0 Transitional//EN">
<HTML><HEAD>
<META content="text/html; charset=iso-8859-1" http-equiv=Content-Type>
<META content="MSHTML 5.00.2919.6307" name=GENERATOR></HEAD>
<BODY
style="FONT: 10pt Abadi MT Condensed Light; MARGIN-LEFT: 2px; MARGIN-TOP: 2px">
<DIV>Are the capacitor locations properly thermal relieved? What is the
orientation into the wave at this location? Could it be that the part is
being thermally shocked due to lack of stress relief in the PCB or orientation
into the wave?</DIV>