Thank you Phil very much. Your studies and comments are very insightful.
It seems "current" solder joint formation technology, dating back over a
thousand or more years, is very reliable and forgiving under almost any
condition, stress, shock, or operational environment. High or relatively low
purity copper, high or low thickness intermetallic compounds, etc. all seem
to have little affect on solder joints, in general. Once a "good" solder
joint is formed, it seems that it should remain in tact for some time. Will
this be true for our "new age" solder joints - as lead free, depending on
the alloy, or not, for a particular application?
Earl Moon
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|