We currently have misplace component at a level of 0.2%. Component placement, solder land proportionality, solderabilty of component terminal and amount of solder was verified to be within specs. Reflow profile was also based in standard settings.
Can you give us some other possible root causes of the above mention problem We are using 0402 SMD and SnPbAg no-clean solder paste.
Leonel Jay J. Manuel
Process Engineer
RF PCC Engineering
Philips Semiconductors Phils. Inc.
Office Tel: (6349) 5430001 to 25
: (632) 8445139 ext. 288
Fax No. : (632) 8445248 / (6349) 5430027
E-mail :[log in to unmask]
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|