This is controversial. Dewetting is caused by myriad non-wettable areas,
most commonly because abrasive particles are implanted in the metal.
IMHO, this means that intermetallic formation is discontinuous and the
joint will be weaker. Whether the loss of strength is important or not
is more academic than real life, but my view is that everything should
be done to maximise strength. Also, if you permit it, where do you start
to draw the line?
Brian
Grant Emandien wrote:
>
> Hi all,
>
> Brian, thanks for your earlier comments.
>
> If a portion of a pad shows evidence of dewetting (some dewetted pad areas
> appear to show base metal) and the solder joint looks good (nice shiny
> fillets), is there reason for concern that these joints may fail at
> temperature excursions (-40°C to +60°C)?
>
> Thanks in advance for responses.
> Grant
>
> **********************************************************************
> Notice:
>
> The information contained in this e-mail (including any attachments) may contain commercially sensitive or confidential information which may be legally privileged and is for the sole use of the intended recipient(s). If you are not, or believe you may not be, the intended recipient, you are hereby notified that any use, dissemination, copying, review, disclosure or action taken in reliance of this e-mail is prohibited and may be unlawful. If you have received this message in error, please notify the sender immediately by reply e-mail and delete all copies of the message.
>
> Any views expressed in this message are those of the individual sender unless expressly stated by the sender to be given on behalf of Tellumat (Pty) Ltd. Tellumat (Pty) Ltd disclaims liability for any unauthorised opinion or representation made by the sender on behalf of Tellumat (Pty) Ltd.
>
> No warranty is given by Tellumat (Pty) Ltd that the integrity or security of this e-mail (including any attachments) has been maintained through transmission, nor that the communication is free of virus, interception or interference.
>
> **********************************************************************
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|