TECHNET Archives

October 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
David Fish <[log in to unmask]>
Date:
Wed, 3 Oct 2001 10:48:40 -0700
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Parts/Attachments:
text/plain (87 lines)
You gave no indication about the material you plan to use or how you plan to
apply the material.  So, this'll be a very rosey picture.

Look in "Metal Finishing" magazine [http://www.metalfinishing.com] for
articles that cover the plant safety [i.e., explosion, fire prevention, fire
containment, fire suppression, OSHA, NFPA, UL, etc], employee safety [i.e.,
PPE, gloves, training, etc], and facilities [i.e., explosion-proof
filtration and exhaust systems, explosion-proof wiring, UL 844 lighting,
safety interlocks and controls, appropriate means of egress, etc.] for paint
spray rooms.

Check with your insurance company, too. Should a bad accident occur, you
might find that you are alone with no insurance to cover the damages. Plus,
you could be liable for negligence.

If you know what is required, then you might want to check out some
auctions. You can get some real good deals if you don't mind taking the
booths apart and moving them. Just know what you're looking at and make sure
they meet your requirements.  When it comes to OSHA, the building
department, fire marshals, etc., they all tend to be at ease once they see
the manufacturer's label staring at them from the header of the booth. Think
about it! There is liability either way.

While switching to VOC-less materials eliminates the flammable solvent
hazard and addresses concerns about organic solvent emissions from an
employee health and environmental perspective, the hazard of the highly
combustible over spray remains.  So, a paint spray booth with sprinkler
protection of the booth interior, as well as the exhaust duct, is required.
And lighting requires taking precautions, because of their potential for
overheating the combustible over spray, even if the electrical fixtures are
explosion proof.

This is no small undertaking.  Consider that there are many fine coating
contractors.

Dave Fish
----- Original Message -----
From: "peter lee" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, September 28, 2001 8:56 AM
Subject: [TN] Setting up conformal coating process


> Hello,
>
> I like to hear your thoughts or experiences on setting
> up a safe and efficient (in particular exhaust,
> floorinconformal coating process g, ESD concerns,
> layout, material storage). Please comment on anything
> you feel critical to process control and success.
>
>
> Peter
>
>
> __________________________________________________
> Do You Yahoo!?
> Listen to your Yahoo! Mail messages from any phone.
> http://phone.yahoo.com
>
> --------------------------------------------------------------------------
-------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> --------------------------------------------------------------------------
-------
>

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2