Good plan. I would add a reminder. Some packages have internal structures to
conduct heat away from active device(s) in the package. These may not be
represented in the dummy component, and can result in an oven profile that
is too cool.
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of <Peter George Duncan>
> Sent: Thursday, October 25, 2001 10:00 PM
> To: [log in to unmask]
> Subject: Re: [TN] Reflow profiling
>
>
>
> I also am involved with high mix, low volume builds, and I try to get one
> board of each type from the fab house that has failed electrical with
> internal shorts or whatever (cheaper than sacrificing a good
> board). I then
> buy in a stack of dummy components from Practical Components or
> Topline and
> populate the profile board with those. I don't bother with discrete
> passives, as they contribute precious little to the thermal mass. The
> thermal profile board is them reflowed using the standard profile supplied
> by the solder manufacturer.
>
> For BGA's and so forth, I then drill a hole up through the board into one
> of the central contacts to take a thermocouple wire, which is bonded in
> place, and add other thermocouples around the board. plug them all into a
> high-temp data logger
>
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|