TECHNET Archives

October 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Eric Dawson <[log in to unmask]>
Date:
Fri, 26 Oct 2001 09:45:09 +0100
Content-Type:
text/plain
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Parts/Attachments:
text/plain (119 lines)
Mike,
In such cases I apply a variable constant.
Happy POETS Day
Regards
Eric Dawson

> -----Original Message-----
> From: Mike Fenner [SMTP:[log in to unmask]]
> Sent: Friday, October 26, 2001 8:33 AM
> To:   [log in to unmask]
> Subject:      Re: [TN] Adjusting the alloy composition in the solderpot
>
> So using your formula that makes Bev about 150 years old percent then, or
> did I miss something.
>
> Happy Friday.
>
> Best regards
>
> Mike
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Lou Hart
> Sent: Thursday, October 25, 2001 5:51 PM
> To: [log in to unmask]
> Subject: Re: [TN] Adjusting the alloy composition in the solderpot
>
>
> Eric, Steve, et al,
>
> I recommend going back to basic calculus and calculating the derivative of
> fraction tin with respect to weight (mass) of tin.
>
> Fraction tin = (Tin mass)/(Tin mass + Lead mass)
>
> You will get (assuming you only want a small change in fraction tin, in
> the
> range of, say, 0.03 or less)
>
> Tin add = (Mass of pot) X (change desired in Fraction Tin)/(Fraction Lead)
>
> On an unrelated matter, let me comment that a number of names like
> Shirley,
> Beverly, and Vivian were used by men until the first half of the past
> century.  Over some time period, women largely took possession of them.
>  Lou Hart
>
>
>
> -----Original Message-----
> From:   Eric Dawson [SMTP:[log in to unmask]]
> Sent:   Thursday, October 25, 2001 2:53 AM
> To:     [log in to unmask]
> Subject:        Re: [TN] Adjusting the alloy composition in the solderpot
>
> Hi All,
> The easiest way to think of this is not the use of a complicated formula,
> but the simple application of percentage.
>
> In the example below, the total weight of tin plus lead is 1500 pounds,
> 61.9% of which is tin. Hence there are 928.5 pounds of tin.
> Add 45 pounds of tin, the total weight is now 1545 pounds of which, 973.5
> pounds is tin. Work out the new percentage of the new total weight and you
> get 63%.
> Ahah, I hear you ask, how do you get to 45 pounds in the first place?
> Well,
> just plug a few numbers into the percentage calculations and see which
> direction it takes you.
> The main thing to remember is that you add the tin addition to the total
> weight as well as the tin content when working out the new percentage.
> Hope this helps
> Regards
> Eric Dawson
>
> --------------------------------------------------------------------------
> --
> -----
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
> Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> --------------------------------------------------------------------------
> --
> -----
>
> --------------------------------------------------------------------------
> -------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
> Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> --------------------------------------------------------------------------
> -------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2