Many fluxes used in board fabrication contain chlorides or bromides.
gary mccauley
-----Original Message-----
From: Cheryl White [mailto:[log in to unmask]]
Sent: Thursday, October 25, 2001 3:37 PM
To: [log in to unmask]
Subject: [TN] Chloride levels
Is there a standard for acceptable levels of chloride on assembled PCBs and
on bare boards? What sources of chlorides exist in a board fabrication
process, and in an assembly process?
We are using a no-clean low-solid flux.
Thanks,
Cheryl White
Manufacturing Engineering
DSC Ltd.
[log in to unmask]
(905) 760-3000 ext. 7228
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|