Brad,
Have you looked at some of the metal tapes that are available? We use an
aluminum one from KIC but I'm sure others have this as well. While it
doesn't quite emulate sticking the thermocouple in solder, the metal mass
when tape this to a solder joint does come pretty close for most profiling
purposes. In our process we do this on the first board out of the oven
which means that board sees a double reflow cycle. We haven't identified
any reliability issues with this but haven't done any long term failure
analysis.
Rick Thompson
Ventura Electronics Assembly
2655 Park Center Dr.
Simi Valley, CA 93065
+1 (805) 584-9858 x-304 voice
+1 (805) 584-1529 fax
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Brad A. Smith
Sent: Thursday, October 25, 2001 8:37 AM
To: [log in to unmask]
Subject: [TN] Reflow profiling
Hello All,
I am with a low volume, frequent changeover contract manufacturer. We are
trying to implement a system where we profile the first assembly of every
new run through our reflow oven. We are currently using high temperature
solder for profiling. If we start to use the high temp solder for this, we
will have to scrap the assemblies. Does anyone have any suggestions for
alternatives to high temp solder? Any suggestions would be greatly
appreciated.
Thank you,
Brad Smith
Process Technician
Badger Electronics Co., Inc.
(262)886-8800
[log in to unmask]
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|