For THT we routinely wave the assemblies. For SMT we never subject the
Tants to wave solder process (bottom of PCB) due to manufacturer
specifications for direct heat over the entire component (note
-entire-). So, we hand solder them in final stages of production.
Tom Parkinson
Jorge Rodriguez wrote:
>
> Technetters,
>
> I have a product that has Tantalum Caps, having them waved would make our
> life easier, the board has some TH components we currently hand solder and
> that could be waved. I know that there might be some reason not to wave
> Tantalums, but I am not sure. Can Tantalum Caps be wave soldered?, Has
> anyone done this?
>
> Any responses would be appreciated
>
> Jorge Rodriguez
> Process Engineer
> Varian Inc
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|