Jorge, we've debated about wave soldering. When such parts were in short
supply (maybe they still are), we decided that, rather than risk any in
wave, we'd hand solder. I called the manufacturer, who only told me that
they were not made to be waved, but a lot of people were doing so. I'm
referring to the axial can style. We had seen fallout at wave before going
to hand. I'm not sure the process couldn't have been tuned to eliminate
the fallout, but there were no parts to risk. Lou Hart
-----Original Message-----
From: Jorge Rodriguez [SMTP:[log in to unmask]]
Sent: Tuesday, October 02, 2001 1:29 PM
To: [log in to unmask]
Subject: [TN] Tantalum Caps
Technetters,
I have a product that has Tantalum Caps, having them waved would make our
life easier, the board has some TH components we currently hand solder and
that could be waved. I know that there might be some reason not to wave
Tantalums, but I am not sure. Can Tantalum Caps be wave soldered?, Has
anyone done this?
Any responses would be appreciated
Jorge Rodriguez
Process Engineer
Varian Inc
------------------------------------------------------------------------
---------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
------------------------------------------------------------------------
---------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|