OK, here is a general question for all you met guys. But I am not sure I
can explain it well enough to be understood!
We all know that tin can be put on iron or we wouldn't have "tin" cans. I
also know it is difficult to put solder on iron. So my question is this: if
one has a tinned iron surface and it is put into molten solder the tin will
be dissolved into the molten solder. I presume when the piece of iron is
withdrawn from the pot, solder will be well adhered to the iron. Is this
because there is a solderable tin/iron intermetallic? What is the main
difference between the tin can process and putting solder directly on iron
that makes one easy to do and the other difficult? This may be a "first
grade" met question, but I don't know the answer. Thanks.
Bev Christian
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|