TECHNET Archives

October 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Date:
Thu, 18 Oct 2001 08:59:41 -0400
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
In-Reply-To:
<A1630D6F27C0D21198AF00805F613595465847@DDLSBS>
Content-Type:
text/plain; charset="iso-8859-1"
From:
Parts/Attachments:
text/plain (65 lines)
If you are the customer, the acceptable defect level is 0, regardless of
class. But seriously, I have seen figures published that indicate visual
inspection to be, at best, 80% effective. I think that number probably
varies a lot based on time of day, day before or after a weekend or holiday,
complexity of the board, etc. Rather than setting an acceptable level, I
would concentrate on having a process that is as robust as possible and
having a system that identifies defects before they get out the door.


Bob


Robert Barr
Manufacturing Engineering
Formation, Inc.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Cathy Killen
Sent: Thursday, October 18, 2001 7:34 AM
To: [log in to unmask]
Subject: [TN] Solder Joint Defects
Importance: High


Could anyone help with this.
When visually inspecting PCBs to class 3, is there an acceptable percentage
of faults missed? Also is there an acceptable defect level considering PPM
with regards to soldered joints.

Cathy Killen
Training Instructor
Smtek Europe Ltd.
The information contained in the E-mail is confidential. It is intended only
for the stated addressee(s) and access to it by any other person is
unauthorised.
The views expressed in this E-mail are those of the author, and do not
represent the views of Smtek Europe, its associates or subsidiaries, unless
otherwise expressly indicated.
Please note: It is your responsibility to scan this E-mail for viruses.

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2