Nope
-----Original Message-----
From: Kathy Kuhlow [mailto:[log in to unmask]]
Sent: Thursday, October 11, 2001 3:38 PM
To: [log in to unmask]
Subject: Re: [TN] failing capacitors
I would think that ,dependent on the thermal ramp rate and the
temperautre spike at the entrance into the solder pot, you could damage
a cap if one lead enters first or if both leads enter the same way and
the part/PCB hasn't ramped up properly or the thermal rate of change
isn't even across the part. Do you have a profiler that you could attach
a thermalcouple wire to and chart what the part is seeing during the
wave process?
Kathy
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------